Unit price in thermoforming is dominated by material, cycle time and freight. Here is the full cost structure and the levers that actually move the number.
The notes below come from day to day production and export work with overseas buyers.
This category covers a family of products rather than a single item. In practice a buyer defines face seal blister packaging by three things: the base resin, the format or dimension, and the performance or certification level it has to meet. Typical options in this category include sheet gauge 0.20 to 0.60 mm; transparent, frosted and coloured; flange width 6 to 12 mm. Materials most often specified are Polystyrene, Recycled PET, Polypropylene, Polyethylene Terephthalate, and the choice between them changes stiffness, temperature resistance, chemical behaviour and price.
In the retail and merchandising sector the decision is usually driven by shelf presentation and print quality, with stack strength as a secondary requirement. Typical end uses include shelf trays, counter displays, pegboard blisters.
Typical values for a general purpose grade are listed below; filled, stabilised and speciality compounds will differ.
| Material | Density | Tensile strength | Service temperature |
|---|---|---|---|
| Polyethylene Terephthalate | 1.35-1.40 g/cm³ | 50-70 MPa | -40°C to 70°C |
| Polypropylene | 0.90-0.91 g/cm³ | 25-40 MPa | -10°C to 100°C |
| Polystyrene | 1.04-1.06 g/cm³ | 30-50 MPa | -20°C to 70°C |
Polypropylene is frequently the default selection here: PP is the lightest mainstream packaging resin and keeps its shape under repeated flexing.
These are the levers buyers can actually influence when negotiating a thermoformed part.
Ask your supplier to quote two gauges and two cavity layouts; the difference shows which lever is worth optimising for your volume.
Beyond the base resin, most suppliers offer UV stabilised, food contact, flame retardant, anti-static and recycled content versions of the same product. Ask which additive package is included, because it is often the difference between a part that lasts three years and one that lasts ten.
Each step below has its own control points, and skipping one of them is where most defects start.
Secondary operations such as printing, welding, machining and assembly are often cheaper to do in the same factory, and they reduce the risk of mismatch between components.
These are the criteria that actually predict whether the part will perform in service.
Send this list to your supplier with the drawing and you will receive comparable quotations from every factory you contact.
Yes. {mat1} is one of our regular materials for this item, and we can supply virgin, modified and certified grades with full traceability. Material certificates and test reports are issued per batch.
Yes. Standard samples are normally free of charge and shipped within three working days; custom samples are charged at cost and credited against the first production order.
We can provide ISO 9001 quality system documentation, material certificates, RoHS and REACH statements, and where applicable food contact, flame retardancy or drinking water approvals. Tell us your target market and we will match the document set.
A new tool typically takes 25 to 45 days depending on cavity count and complexity, followed by T1 samples within one week. Existing tools can usually start production within 10 to 15 days of order confirmation.
Standard production tolerance follows the relevant ISO or DIN tolerance class for the process; tighter tolerances are possible after machining or grinding, but they add cost. Define the tolerance only on the functional dimensions.
If you are planning a new retail and merchandising project, send us your drawing, annual volume and target properties, and we will come back with a material proposal, a tooling plan and a budget quotation.
Rubber & Plastics © 2026 All Rights Reserved. Yingnet.com — Global B2B trade platform for rubber & plastics manufacturers.